Technical Support

White Chlorinated Rubber/Alkyd Lacquer
Time: 2019-12-12

Formulation:

  I Parts (w/w) II Parts (w/w)
5~20mpa.S Chlorinated Rubber - -
Medium-oil Soy Alkyd (70%) 8.5 8.9
Long-oil Linseed Alkyd (70%) 30.4 27.0
Titanium Dioxide (Rutile) 18.4 19.40
Cobalt Naphthenate 0.2 0.2
Lead Naphthenate 0.4 0.4
MEKO 0.1 0.1
Petroleum Solvent 8.0 11.0
Aromatic Solvent 34.0 33.0
Total 100 100